nanoindentation sentence in Hindi

"nanoindentation" meaning in Hindi  nanoindentation in a sentence  

Examples

  1. Nanohardness refers to the " hardness " measured by " nanoindentation " method when the depth of " indentation " is expressed in " nanometer " . ( less than one micron ) If the average depth is over one " micron ", the term " microhardness " should be used despite the measurement was done by " nanoindentation " method.
  2. Nanohardness refers to the " hardness " measured by " nanoindentation " method when the depth of " indentation " is expressed in " nanometer " . ( less than one micron ) If the average depth is over one " micron ", the term " microhardness " should be used despite the measurement was done by " nanoindentation " method.